Vancouver - BAROYECA GOLD & SILVER INC. (TSXV: BGS) (the 'Company') is pleased to announce assay results from the first group of channel samples taken at 1m intervals over the first 18m of exploratory tunnel on Vein #2 at its Santa Barbara gold project in Bolivar, Colombia.

The Santa Barbara exploratory tunnel has been driven for 150m following a continuous shoot in a gold bearing vein (Santa Barbara vein or Vein #1). Vein #2 is parallel to Vein #1 and was intersected after a 40m northwest directed crosscut tunnel perpendicular to Vein #1.

Channel sampling started at meter 40 from where the exploratory crosscut tunnel intersected Vein #2 under existing artisanal mining works mapped on surface. The exploratory tunnel was driven for 9m to the southwest and 8.5m to the southeast following the vein from the crosscut tunnel where it was intersected.

Sample collection method

The mining method employed at the tunnel consists of splitting the vein from the barren wall rock, separating and collecting the vein material with a minimum of wall rock shoulder attached. The vein material from the tunnel is then bagged at the tunnel portal in woven plastic bags and individually weighed until an approximate nominal 15-ton batch sized sample is completed. Samples are then loaded in random order in a truck and taken to the Santa Barbara pilot gold processing plant. At the plant site, sample bags are dumped in random order to pass through a first stage of crushing to 2 inch and then a second stage of crushing to 0.5 inch particle size. Crushed material is then stored in a bin with a vibrating door that self-feeds the primary ball mill. Crushed material is then sent to the primary ball mill (>40% passing 150 mesh) and secondary ball mill (>60% passing 200 mesh) connecting with the three 15m3 cyanide leaching talks where the pulp is agitated before adding any reagent for homogenization purposes.

The pilot plant does not have any gravity separation stage or flotation system therefore there is no loss of material in the process and the sample pulp once reaches the cyanide leaching tanks can be considered the entire sample and the sample being homogenized. A 1 kg head grade sample is then collected from the tank before the cyanide leaching process can start.

About Baroyeca Gold & Silver Inc.

Baroyeca Gold & Silver Inc. is a mineral exploration company focused on high-grade silver and gold projects located in Colombia. Baroyeca's flagship asset is the high-grade Atocha Silver-Gold Project located in Tolima Department, Colombia. The Company also holds an option to acquire a 100% interest in the Santa Barbara Property, Bolivar Department, Colombia, which is renowned for its high-grade gold mineralization and vein density. Current exploration activities on the Santa Barbara Property involve the bulk sampling of vein structures, which material then feeds into a trial production facility which has consistently been producing gold for over a year. The revenue from the sale of produced gold defrays part of the operating costs. The Company is planning to expand these activities.

The Company's Board and senior management are committed to creating shareholder value through the discovery process, careful allocation of capital, and environmentally and socially responsible mineral exploration.